Class C25/30 designates a concrete whose characteristic compressive strength at 28 days is 25 MPa measured on a cylinder and 30 MPa measured on a cube: these are two ways of measuring the same concrete quality. The older designation B25, still common in Moroccan specifications (CPS) drafted according to the BAEL, generally refers to a strength of 25 MPa at 28 days on a cylinder, close to a C25/30. Always ask for the reference standard to be stated.
Reading a concrete class
In the European designation (EN 206 standard, Eurocode 2), the letter C stands for "concrete"; the first number is the strength on a 15 × 30 cm cylinder, the second on a 15 cm cube, both in MPa at 28 days. The cube gives a higher value than the cylinder for the same concrete, hence the two figures. With the BAEL, the design strength is written fc28, measured on a cylinder. Note: in other systems of standards, a letter B followed by a number may designate a cube strength; if in doubt, ask for clarification in writing.
| Class | Cylinder (MPa) | Cube (MPa) | Typical use (indicative) |
|---|---|---|---|
| C20/25 | 20 | 25 | Lightly stressed reinforced concrete, ground slabs |
| C25/30 | 25 | 30 | Typical structure of a villa or small building |
| C30/37 | 30 | 37 | More heavily stressed or exposed structures, swimming pools, car parks |
| C35/45 | 35 | 45 | Demanding structures, aggressive environments |
Strength class and exposure class
Strength is not the only criterion. Durability depends on the environment: dry interior, exterior, contact with water, aggressive soils, marine environment. The EN 206 standard defines exposure classes (XC, XS, XD, XA…) which impose a minimum cement content, a maximum water/cement ratio and sometimes a minimum strength. A swimming pool, a tank or a foundation in aggressive soil may thus require a higher-performance concrete than the strength calculation alone would require. The choice of class and of cover go hand in hand.
Actually getting the specified class
- Ready-mixed concrete: order the strength class, the exposure class and the consistency, and check the delivery note of each truck.
- Site-mixed concrete: a well-executed mix with 350 kg of cement per m³ commonly achieves a class of around C25/30, but without any guarantee; the quality of the aggregates and the amount of water change everything (see concrete mix proportions).
- Test specimens: take specimens during major pours and have them crushed by a laboratory at 7 and 28 days.
- No water added on site: this is the leading cause of concrete falling below its class.
The role of the engineering firm
The engineering firm sets the strength class and exposure class of each element in its design calculations and the specifications. It can require tests and interpret the results: concrete that does not reach its class means the element must be recalculated, or even strengthened.
Frequently asked questions
What does C25/30 mean?
It is a concrete whose characteristic strength at 28 days is 25 MPa on a cylinder and 30 MPa on a cube, according to the EN 206 standard.
Are B25 and C25/30 the same thing?
In a specification drafted according to the BAEL, B25 generally designates a concrete of 25 MPa on a cylinder at 28 days, close to a C25/30. Ask for the reference standard to be stated, as other systems measure on cubes.
Which concrete class for a villa?
A C25/30 class is common for the structure of a villa; the engineer may require more for swimming pools and buried or exposed structures.
A project in the pipeline?
SIGMA ICC designs reinforced concrete, electrical, plumbing and HVAC systems and supervises sites for villas, riads, hotels and shops.
Sources : Travail Industrie, classes de résistance du béton · AFGC, caractéristiques mécaniques des bétons · Holcim, la norme béton EN 206.